サプライヤーと連絡する

Ms. Susan Niu
伝言を残すお支払い方法の種類: | L/C,T/T,Paypal,Western Union |
---|---|
Incoterm: | FOB,CFR,CIF |
最小注文数: | 500 Kilogram |
納期: | 20 天数 |
基本情報
モデル: DD-EC23
材料: 積層材
使用法: 包装フィルム, テキスタイル・アパレル, ギフト包装, 業界
処理タイプ: 多重押出
透明性: 半透明
特徴: モイスチャープルーフ
硬度: 柔らかい
Width: 300mm-2500mm
Treatment: Glossy,matt
Length: 3000m-18000m
Thickness: 12-50micron
Roll Core: 3inch,6inch
Samples: A4free Samples
Additional Info
包装: ロールごとにカートンで梱包する
生産高: 3000mt
ブランド: DADAO
輸送方法: Ocean,Land,Air
原産地: 中国
供給能力: 3000mt
認証 : CE,SGS
製品の説明
熱ラミネート用EVAコートBOPPフィルム
必要な温度に達すると操作が簡単になり、特別な技術は必要ありません。
DECRIPTION OF PRODUCTS
|
|
Environmentally friendly |
It is environmentally friendly, non-hazardous to health and safe to use as no toxic gases or volatile content is emitted. Safety in laminating process as no solvent based adhesive is used. |
High function |
Compared with other solvent lamination, our film is better in clarity and bonding. Strong ability of absorbing powder. It prevents lamination from being pressed, bubbled and shredded off easily. Matt thermal lamination film is good for spot UV and hot stamping. |
Efficient and energy-saving |
Production cost is reduced substantially as there is no film wastage, mixture of adhesive solvent, and no UV heating lamp is required. |
Adaptable to different kinds of machines |
This film is recommended to be used in dry laminator. Small adjustments need to be made to the machine if the film is used in wet laminator. |
Process Parameter |
Equipment for laminating film: dry and wet film laminator Temperature: Normal:85~100°C Special:100~110 °C Roller pressure:10~18Mpa Speed:8~50m/min Remarks: Special laminations refer to those with thicker ink, solid color, high moisture content and bigger size paper. |
Application manually |
1. Adjust roller pressure and temperature according to different types of paper and ink. 2. When using the film for the first time or changing to other sizes, we recommend a small trial volume before going into fully mass lamination. 3. The following situation will affect the quality of the film during lamination. 1. When using metal ink. 2. When the ink contains too much wax, dried oil, adhesive, and silicon additive. etc. 3. When the ink is too thick. 4. When the ink is not completely dry. 5. When the paper contains too much moisture. 6. When there is too much powder. |
製品グループ : BOPP積層フィルム > BOPP Thermal Film